During processing Ceramer can withstand very high temperatures even over long periods.
|
|
At 320 °C over a period of 12 hours the weight loss is less than 1% (curve d).
|
|
At 360 °C over a period of 12 hours the weight loss is only 4% (curve b).
|
|
Curve a shows the weight loss at the recommended pre-treatment temperature of 375 °C, if Ceramer is used in free sintering of large volume parts. The drying duration is usually 330 minutes. The drying atmosphere is circulating air in a covered but vented container.
|